Care Precision Industrial Co., Ltd

Call Directions Website Contact the business

Care Precision Industrial Co., Ltd ONE-STOP SOLUTION FOR TOOLING AND METAL

2026/11/06

How do you form a shallow tray with a clean, consistent rim?💯

This four-station stamping sequence shows the logic:
1. Initial drawing establishes the basic tray shape.
2. Trimming removes excess material and defines the profile.
3. Flanging forms the rim and corner transitions.
4. Restriking calibrates the final shape for repeatable production.

The process looks simple—but stable material flow and controlled geometry make the difference.

2026/11/05

Rolling a ball-head terminal is not a one-stroke operation.
A stable spherical profile comes from staged forming: pre-forming, controlled side curls, progressive rolling, and final restrike calibration.

The goal is simple—control material flow, protect the profile, and turn a complex terminal into repeatable production.

2026/11/03

There is no universal answer. The right forming mechanism depends on part geometry, bend angle, forming access, springback control, cycle time, and maintenance requirements.Good die design is not about choosing the most complex structure—it is about using the simplest mechanism that delivers stable and repeatable parts.Which structure would you choose?

2026/11/02

Sharing one process from CAE analysis to stable aluminum mass production.😊

Before tool tryout, CAE was used to evaluate material flow, wall thinning, wrinkling, and splitting risk. The progressive deep-drawing die then forms the part through drawing followed by reverse redrawing—controlling the material step by step.

Simulation guides the process. Production proves the result.

2026/10/29

Turning vertical press motion into horizontal forming force.

This side-push forming die first preforms the flat blank into a U-shaped profile. Near bottom dead center, cam-driven slides move inward from both sides to complete the negative-angle bends.

As the die opens, spring-loaded slides retract for easy part release.

The mechanism looks simple—but precise timing between preforming, side forming, and slide return is the key.

2026/10/19

Round-tube cutoff dies look simple—until feeding and part release become the bottleneck.

This design uses a cam-driven lateral slide to locate and support the tube. The profiled cutoff punch completes the shear in one press cycle, while return springs retract the slide for the next feed.

With tube-specific inserts and correctly set clearance, the concept can be adapted to different tube diameters.

3D motion explained. Real production verified.

2026/10/16

Six die layouts. One wall-ironing principle.

This animation shows six tooling configurations for wall ironing. In each design, a pre-drawn cup is forced through an ironing die with a radial punch-to-die clearance smaller than the incoming wall thickness.

The result: a thinner wall and a taller shell.

Regardless of the tooling layout, stable production depends on controlled reduction, accurate alignment, effective lubrication, and high-quality tool surfaces.

Which layout would you choose for production?

2026/10/14

How do you control flatness in dense-perforation tooling?

Dense holes. Hidden stress. Visible warpage.

In high-density perforation punching, repeated shearing and local bending can build residual stress across a flat sheet, gradually pulling it out of plane.

The solution shown here uses a slightly convex, crowned die face to introduce controlled counter-bending. This helps offset accumulated deformation and improve sheet flatness.

A small geometry change—but one that must be tuned to the material, thickness, and hole pattern.

2026/10/07

What is the new stamping tool first-tryout common problem?

New die. First tryout. Multiple defects. Multiple defects.

Slug carry-up, broken punches, excessive burrs, galling, deformation, and unstable dimensions may look related—but each can have a different root cause.

Stable production starts with a disciplined process: identify the symptom, verify the cause, and apply the right corrective action.

Which die-tryout issue costs your team the most time?

🎄Season’s Greetings from Care Precision! ✨As we reflect on this year, we’re deeply grateful for the trust and collaborat...
2025/12/25

🎄Season’s Greetings from Care Precision! ✨
As we reflect on this year, we’re deeply grateful for the trust and collaboration of our partners.
Our commitment — Care in every connection, Precision in every part — guides us every day.
Wishing you and your team joy, rest, and a bright New Year ahead! 🥂
Thank you for partnering with us.

Address

402760
Chongqing Shi
Building 13, No. 568, JinJian Road, Biquan Street Bishan District

Opening Hours

Monday 08:00 - 20:00
Tuesday 08:00 - 20:00
Wednesday 08:00 - 20:00
Thursday 08:00 - 20:00
Friday 08:00 - 20:00
Saturday 08:00 - 20:00
Sunday 08:00 - 20:00

Telephone

+862341555595

Alerts

Be the first to know and let us send you an email when Care Precision Industrial Co., Ltd posts news and promotions. Your email address will not be used for any other purpose, and you can unsubscribe at any time.

Contact The Business

Send a message to Care Precision Industrial Co., Ltd:

Shortcuts

Share

Nearby businesses